PA250013.JPG
Painting epoxy on a seam. I use cheap paint brushes because you can't reuse them.
PA250015.JPG
Wetting out the fiberglass.
PA250016.JPG
Wetting out the fiberglass.
PA250019.JPG
Applying mylar film. Epoxy doesn't stick to the mylar. Weight applyed will hold the joint flat.
PA250020.JPG
Remove bubbles under mylar
PA260001.JPG
Scrapping excess epoxy
PA260002.JPG
Epoxy seepage from other side
PA260004.JPG
Level surface prior to applying fiberglass.
PA270001.JPG
Deck pieces.
PA270002.JPG
Deck pieces.
PA270003.JPG
Deck pieces.
PA270004.JPG
Reinforcement plate.
PA270005.JPG
Cutting reinforcement plates.
PA270006.JPG
Layout reinforcement plates.
PA270007.JPG
Mixing wood flour and epoxy. This creates a "glue".
PA270008.JPG
Paint on wood flour and epoxy mixture
PA270009.JPG
Glue reinforcement plate in place
PA270010.JPG
Place weights on reinforcement plates.
PA270011.JPG
Reinforcement plate close-up.
PA270012.JPG
Cut stitching wires.