PB060005.JPG
Side seam.
PB060006.JPG
Rolling on saturation coat. This seals the wood in preparation for the fiberglass.
PB060009.JPG
Saturation coat completed.
PB060010.JPG
Saturation coat.
PB070001.JPG
Applying fiberglass after saturation coat has cured.
PB070002.JPG
Preparing epoxy.
PB070003.JPG
Pumping epoxy. The halogen light is just for lighting the area. The heat from the lamp warms the epoxy which makes it thinner.
PB070004.JPG
Rolling on epoxy over fiberglass.
PB070005.JPG
Competed fiberglass.
PB070006.JPG
Stern fiberglass.
PB070007.JPG
Fiberglass weave.
PB070008.JPG
Fiberglass weave.
PB080001.JPG
Keel reinforcement strip.
PB080002.JPG
Reinforcement strip over butt seem.
PB090003.JPG
Fiberglassed bow.
PB090005.JPG
Reinforcement strip looking at bow.
PB120006.JPG
Reinforcement strip looking at stern.
PB120007.JPG
Completed hull fiberglassing.
PB120008.JPG
Right side up.
PB120009.JPG
Loose fitting deck pieces.